ROD,PREMIUM,RND,BRAZING,CU,0.31 LB/IN
- Exposure to pressured steam can also result in accelerated corrosion
- For copper-base alloys, such as brass or bronze, the joints should be fluxed
- Should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints
- Should not be used where the joints are exposed to sulfur compounds, especially in gases or oils at temperatures above normal room temperature
- The self fluxing property of this filler metal is effective on copper only